Short answer

Degrease the part at 10 to 12V DC, then stroke the nickel pen over it at 5 to 6V. Nickel plates directly onto copper; steel, brass and other metals get a copper flash first. A standard nickel pen deposits about 0.4 µm in 2 minutes on a 1 in² area and builds to 1.5 to 1.8 µm. The pen is $70.

This job is done with brush plating, a form of selective plating that puts metal only where the pen tip touches.

What a nickel pen is used for

  • The underlayer under gold on connector pins, edge connectors and PCB gold fingers
  • The required base under rhodium and palladium
  • Restoring worn nickel on machinery components and contact surfaces
  • Corrosion-protection touch-up on industrial equipment

What nickel will plate onto

The nickel pens plate over copper. Any other metal gets a copper flash with the Copper pen (PL-1010) first, and stainless steel is cleaned with its own degreaser.

Nickel plating sequence by base metal
Base metalSequence
CopperDegrease, then nickel
Brass, steel or zinc die-castDegrease, copper flash, then nickel
Stainless steelStainless degreaser, copper flash, then nickel
AluminumNot supported by the Micro-Metallizer system

Step by step

  1. 01

    Remove oxide and discoloration

    If the surface is discolored or oxidized, polish it with a fine metal polish until the oxide is gone, then wipe it clean with a lint-free cloth.

  2. 02

    Degrease at 10 to 12V

    Set the supply to 10 to 12V and use the Absorbent / Degreaser pen (PL-1002). Connect the part to the negative (−) lead of the power supply and the pen to the positive (+) lead. Hold the pen so the whole tip touches the surface, and move it lightly back and forth in a slow stroke. Small bubbles form as oil and grease come off. Wipe the area clean with a cloth when done. Stainless steel takes the Stainless Steel Degreaser pen (PL-1014) instead.

  3. 03

    Copper flash, on anything that is not copper

    Plate a thin copper layer with the Copper pen (PL-1010) at 6 to 8V. Wipe clean with a cloth. Skip this step on copper.

  4. 04

    Plate nickel at 5 to 6V

    Set the supply to 5 to 6V and switch to the Nickel pen (PL-1006). Connect the part to the negative (−) lead of the power supply and the pen to the positive (+) lead. Hold the pen so the whole tip touches the surface, and move it lightly back and forth in a slow stroke.

  5. 05

    Build to thickness

    A standard nickel pen deposits about 0.4 µm in 2 minutes and 0.6 µm in 3 minutes on a 1 in² area, up to 1.5 to 1.8 µm. Keep working the area to build more.

  6. 06

    Wipe clean

    Wipe the part with a clean, soft cloth. If a finish goes on top, switch pens and plate it now.

Order the parts for this job

In stock. Ships same day on orders placed by 2 PM ET on business days.

See every pen and kit in the store →

Standard, heavy-duty or black nickel

Use the heavy-duty pen for a thicker underlayer under production gold or rhodium work. Black nickel plates the same way as nickel, at a higher voltage, and leaves a dark, low-reflectivity finish.

Micro-Metallizer nickel pens. Deposit figures are on a 1 in × 1 in copper surface, from the catalog.
PenCatalog no.PriceVoltage (DC)2 minutes3 minutesMaximum
NickelPL-1006$705 to 6V0.4 µm0.6 µm1.5 to 1.8 µm
Nickel HeavyPL-1020$1205 to 6V0.8 µm1.2 µm3 to 3.6 µm
Black NickelPL-1007$708 to 10V0.5 µm0.6 µm1.5 to 1.8 µm

What you need

The Nickel pen ($70), the Absorbent / Degreaser pen ($65), the power supply ($220) and connector cables ($20) come to $375. Add the Copper pen ($65) if you plate anything other than copper.

If the nickel is going under gold, the Contact Repair Kit ($400) is the better buy: it has the power supply, cables, degreaser and nickel pens, plus a 24K gold pen.

Frequently asked questions

What voltage do you use for nickel plating with a pen?

5 to 6V DC for the Nickel and Nickel Heavy pens, with the part on the negative lead and the pen on the positive lead. Black Nickel runs at 8 to 10V. Degreasing beforehand runs at 10 to 12V.

Can you nickel plate steel with a pen?

Yes, with a copper flash first. Degrease, plate a thin copper layer with the Copper pen, then plate nickel.

Do I need nickel under gold?

On copper, yes. Gold pens plate over gold, nickel or silver, not bare copper, so nickel goes down first.

How thick is brush-plated nickel?

A standard nickel pen builds up to 1.5 to 1.8 µm, at about 0.4 µm in 2 minutes on a 1 in² area. The heavy-duty pen builds up to 3 to 3.6 µm.

How much area does one nickel pen cover?

Each pen holds 10 ml of concentrated solution and plates roughly 300 square inches.

Shop the parts in this guide

Plating PenPL-1006

Nickel Plating Pen

Plate nickel over copper surfaces. Apply copper flash first on non-copper substrates. Essential underlayer for many plating sequences.

$70.00
Plating KitPL-1000C

Contact Repair Kit

Complete repair kit for electronic component restoration. Includes power supply, connector cables, Absorbent, Nickel, and 24K Gold pen.

110V / 220V · choose in cart

$400.00
Heavy-Duty PenPL-1020

Nickel Heavy Duty Pen

Heavy-duty nickel pen for thick nickel deposits. Used as a heavy underlayer for gold, rhodium, and other precious metal platings.

$120.00
Plating PenPL-1010

Copper Plating Pen

Plate copper over any metallic surface (not aluminum or chromium). Used as an intermediate flash layer for other platings.

$65.00

Not sure which pens your part needs?

Tell us the substrate and the finish you need. Our team will tell you the sequence.

Related guides